Title: Maintenance Management of Turbine Generator Foundation Affected by Alkali–Silica Reaction

Author(s): Ryosuke Manabe, Hiroshi Kawae, Kiyoshi Ogawa, Masayuki Matsuura

Publication: JCI

Volume: 14

Issue: 9

Appears on pages(s): 590 - 606

Keywords:

DOI: 10.3151/jact.14.590

Date: 1/1/2016

Abstract: