Title:
Fatigue Analysis of RC Slabs Reinforced with Plain Bars Based on the Bridging Stress Degradation Concept
Author(s):
Ahmed Attia M. Drar, Takashi Matsumoto
Publication:
JCI
Volume:
14
Issue:
1
Appears on pages(s):
21 - 34
Keywords:
DOI:
10.3151/jact.14.21
Date:
1/1/2016
Abstract: