Title: Simulation of Humidity Fields in Concrete: Experimental Validation and Parameter Estimation

Author(s): Mateus A. Oliveira, Miguel Azenha, Paulo B. Lourenço

Publication: JCI

Volume: 13

Issue: 4

Appears on pages(s): 214 - 229

Keywords:

DOI: 10.3151/jact.13.214