Title: Meso-scale Mechanical Model for Mortar Deformation under Freeze Thaw Cycles

Author(s): Fuyuan Gong, Evdon Sicat, Tamon Ueda, Dawei Zhang

Publication: JCI

Volume: 11

Issue: 2

Appears on pages(s): 49 - 60

Keywords:

DOI: 10.3151/jact.11.49

Date: 1/1/2013