International Concrete Abstracts Portal

  


Title: Characteristics of the Surface Air Permeability Test and the Evaluation of Quality Variation in Cover Concrete due to Segregation of Concrete

Author(s): Yoshitaka Kato

Publication: JCI

Volume: 11

Issue: 11

Appears on pages(s): 322 - 332

Keywords:

DOI: 10.3151/jact.11.322

Date: 1/1/2013

Abstract: