Title:
Application of Electrical Treatment to Alteration of Cementitious Material due to Leaching
Author(s):
Katsufumi Hashimoto, Nobuaki Otsuki, Tsuyoshi Saito, Hiroshi Yokota
Publication:
JCI
Volume:
11
Issue:
3
Appears on pages(s):
108 - 118
Keywords:
DOI:
10.3151/jact.11.108
Date:
1/1/2013
Abstract: