Title: Effect of the Key Mixture Parameters on Tortuosity and Permeability of Concrete

Author(s): Shamsad Ahmad, Abul Kalam Azad, Kevin F. Loughlin

Publication: JCI

Volume: 10

Issue: 3

Appears on pages(s): 86 - 94

Keywords:

DOI: 10.3151/jact.10.86

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access