International Concrete Abstracts Portal

  


Title: Tidal Water Effect on the Hybrid Cathodic Protection Systems for Marine Concrete Structures

Author(s): Jin-A Jeong, Chung-Kuk Jin, Won-Sub Chung

Publication: JCI

Volume: 10

Issue: 12

Appears on pages(s): 389 - 394

Keywords:

DOI: 10.3151/jact.10.389

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.