Title: Optimum Surface Protection System with Silane Type Water Repellents

Author(s): Akira Hosoda, Yoshinori Matsuda, Kaoru Kobayashi

Publication: JCI

Volume: 8

Issue: 3

Appears on pages(s): 291 - 302

Keywords:

DOI: 10.3151/jact.8.291