International Concrete Abstracts Portal

  


Title: Salt Weathering in Residential Concrete Foundations Exposed to Sulfate-bearing Ground

Author(s): Natsuki Yoshida, Yoshio Matsunami, Masaru Nagayama, Etsuo Sakai

Publication: JCI

Volume: 8

Issue: 2

Appears on pages(s): 121 - 134

Keywords:

DOI: 10.3151/jact.8.121

Date: 1/1/2010

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  