Title: Experimental Investigation on Shear Cracking Behavior in Reinforced Concrete Beams with Shear Reinforcement

Author(s): Mohamed Zakaria, Tamon Ueda, Zhimin Wu, Liang Meng

Publication: JCI

Volume: 7

Issue: 1

Appears on pages(s): 79 - 96

Keywords:

DOI: 10.3151/jact.7.79