Title: Experimental Behaviour of Carbon FRP Reinforced Concrete Beams at Ambient and Elevated Temperatures

Author(s): Muhammad Masood Rafi, Ali Nadjai

Publication: JCI

Volume: 6

Issue: 3

Appears on pages(s): 431 - 441

Keywords:

DOI: 10.3151/jact.6.431