Title: Simulation of Steel Corrosion in Concrete Based on the Model of Macro-Cell Corrosion Circuit

Author(s): Tsuyoshi Maruya, Hitoshi Takeda, Kenichi Horiguchi, Satoru Koyama, Kai-Lin Hsu

Publication: JCI

Volume: 5

Issue: 3

Appears on pages(s): 343 - 362

Keywords:

DOI: 10.3151/jact.5.343

Date: 1/1/2007

Abstract:


Japan Concrete Institute, International Partner Access