Title: Particle Arrangements in Freshly-Mixed Mortars: Basis for Modeling
Author(s): Sidney Diamond
Publication: JCI
Volume: 5
Issue: 3
Appears on pages(s): 277 - 283
Keywords:
DOI: 10.3151/jact.5.277
Date: 1/1/2007
Abstract:
Japan Concrete Institute, International Partner Access