Title: Development of Self-Healing System for Concrete with Selective Heating around Crack

Author(s): Tomoya Nishiwaki, Hirozo Mihashi, Byung-Koog Jang, Kazuaki Miura

Publication: JCI

Volume: 4

Issue: 2

Appears on pages(s): 267 - 275

Keywords:

DOI: 10.3151/jact.4.267

Date: 1/1/2006

Abstract:


Japan Concrete Institute, International Partner Access