International Concrete Abstracts Portal

  


Title: Analytical Hydration Model for Filler Rich Binders in Self-compacting Concrete

Author(s): Anne-Mieke Poppe, Geert De Schutter

Publication: JCI

Volume: 4

Issue: 2

Appears on pages(s): 259 - 266

Keywords:

DOI: 10.3151/jact.4.259

Date: 1/1/2006

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer