Title: Development of Simulation Model of Chloride Ion Transportation in Cracked Concrete

Author(s): Ema Kato, Yoshitaka Kato, Taketo Uomoto

Publication: JCI

Volume: 3

Issue: 1

Appears on pages(s): 85 - 94

Keywords:

DOI: 10.3151/jact.3.85

Date: 1/1/2005

Abstract: