Title: Stress-Strain Model of Concrete Damaged by Freezing and Thawing Cycles

Author(s): Muttaqin Hasan, Hidetoshi Okuyama, Yasuhiko Sato, Tamon Ueda

Publication: JCI

Volume: 2

Issue: 1

Appears on pages(s): 89 - 99

Keywords:

DOI: 10.3151/jact.2.89

Date: 1/1/2004

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  