Title: Nonlinear Analysis of RC Structural Members Using 3D Lattice Model
Author(s): Tomohiro Miki, Junichiro Niwa
Publication: JCI
Volume: 2
Issue: 3
Appears on pages(s): 343 - 358
Keywords:
DOI: 10.3151/jact.2.343
Date: 1/1/2004
Abstract:
Japan Concrete Institute, International Partner Access