Title:
Microstructure Changes in Autoclaved Aerated Concrete during Carbonation under Working and Accelerated Conditions
Author(s):
Fumiaki Matsushita, Yoshimichi Aono, Sumio Shibata
Publication:
JCI
Volume:
2
Issue:
1
Appears on pages(s):
121 - 129
Keywords:
DOI:
10.3151/jact.2.121
Date:
1/1/2004
Abstract: