Title: Properties of Hybrid Fiber Reinforced Cement - based Composites

Author(s): Atsushi Kawamata, Hirozo Mihashi, Hiroshi Fukuyama

Publication: JCI

Volume: 1

Issue: 3

Appears on pages(s): 283 - 290

Keywords:

DOI: 10.3151/jact.1.283