Title: Rheological Behaviour of Alkali-Activated Slag Concrete

Author(s): Francisca Puertas, María del Mar Alonso, Manuel Torres-Carrasco, Belen González Fonteboa, Iris González Taboada, Gemma Rojo, and Fernando Martínez-Abella

Publication: Symposium Paper

Volume: 320

Issue:

Appears on pages(s): 6.1-6.12

Keywords: Alkali activated concretes; compressive strength; mixing time; rheology

DOI: 10.14359/51701044

Date: 8/1/2017

Abstract:
This study compared waterglass- and NaOH-activated slag concrete (AASC) rheology to the behaviour in OPCC concrete. The effect of mixing time on fresh concrete rheology was also assessed. A rotational rheometer was used to apply shear stress to the materials to determine static and dynamic yield stress at 15, 30, 45 and 60 min of age. Concrete strength and porosimetry were determined to relate rheology to hardened concrete behaviour. The results indicate that slump and rheological behaviour of OPCC and AASC are different, scpecially when the alkaline activator is waterglas (AAS WG). The mixing protocol appeared to affect concrete rheology (fresh behaviour) more than its strength (hardened behaviour). In AASC WG, both rheological and mechanical behaviour improved at longer mixing times.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.