Title: Measuring the Cracking Potential of Shotcrete

Author(s): Sébastien Girard, Marc Jolin, Benoit Bissonnette, and Jean-Daniel Lemay

Publication: Concrete International

Volume: 39

Issue: 8

Appears on pages(s): 44-48

Keywords: ring test, stress, time, variability

DOI: 10.14359/51700958

Date: 8/1/2017

Abstract:
A recent research project was conducted to develop a suitable test method for evaluating the shrinkage cracking sensitivity of shotcrete mixtures. The experimental approach and an overview of the testing program are summarized, and the challenges of producing realistic and homogenous test specimens are discussed.

Related References:

1. Hossain, A.B., and Weiss, J., “Assessing Residual Stress Development and Stress Relaxation in Restrained Concrete Ring Specimens,” Cement and Concrete Composites, V. 26, No. 5, July 2004, pp. 531-540.

2. Hossain, A.B., and Weiss, J., “The Role of Specimen Geometry and Boundary Conditions on Stress Development and Cracking in the Restrained Ring Test,” Cement and Concrete Research, V. 36, No. 1, Jan. 2006, pp. 189-199.

3. Moon, J.H., and Weiss, J., “Estimating Residual Stress in the Restrained Ring Test under Circumferential Drying,” Cement and Concrete Composites, V. 28, No. 5, May 2006, pp. 486-496.

4. Courard, L.; Bissonnette, B.; and Garbacz, A., “Fundamental Approach for the Concept of Concrete Repair Compatibility,” International Conference on Concrete Repair, Rehabilitation and Retrofitting IV, CRC Press, Boca Raton, FL, 2016, 164 pp.

5. AASHTO T 334-08, “Standard Method of Test for Estimating the Cracking Tendency of Concrete,” American Association of State and Highway Transportation Officials, Washington, DC, 2008, 6 pp.

6. ASTM C1581/C1581M-09, “Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restreined Shrinkage,” ASTM International, West Conshohocken, PA, 2009, 7 pp.

7. “CP-60(09): Craftsman Workbook for ACI Certification of Shotcrete Nozzleman,” American Concrete Institute, Farmington Hills, MI, 2009, 126 pp.

8. Girard, S., “Étude du Bilan Déformationnel des Bétons Projetés,” MS thesis, Laval University, Quebec City, QC, Canada, 2014, 174 pp. (in French)

9. Bažant, Z., and Oh, B.H., “Crack Band Theory for Fracture of Concrete,” Materials and Structures, V. 16, No. 3, May 1983, pp. 155-177.

10. Broek, D., Elementary Engineering Fracture Mechanics, Springer Netherlands, 1982, 469 pp.

11. Modjabi-Sangnier, F., “Approche Quantitative de la Notion de Compatibilité des Bétons de Réparation Autoplaçants,” PhD dissertation, Laval University, Quebec City, QC, Canada, 2010, 235 pp. (in French)




  

Edit Module Settings to define Page Content Reviewer