Effects of Intergrinding 12% Limestone with Cement on Properties of Cement and Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Intergrinding 12% Limestone with Cement on Properties of Cement and Mortar

Author(s): James Mohammadi, Warren South

Publication: CCAA

Volume: 14

Issue: 5

Appears on pages(s): 215-228

Keywords: General Purpose (GP) cement; Limestone cement; Mortar; Mortar Sulfate Expansion; Mortar Drying Shrinkage; Mortar Compressive strength

DOI:

Date: 5/1/2016

Abstract:
This paper provides information concerning the results of test programme to investigate the properties and performance of Type General Purpose (GP) cement containing up to 12% limestone. Cement properties, including chemical and physical properties and mortar properties, such as compressive strength, drying shrinkage, and sulfate expansion were investigated comprehensively for effects of introducing higher limestone content to General Purpose (GP) cement. Test results showed that there is no significant effect on most properties due to increasing the limestone addition in cement from 7.5% to a maximum of 12%.