Title: A New AIJ standard for Seismic Capacity Calculation: Recent Advances in Beam-Column Joint Design and Seismic Collapse Simulation on Reinforced Concrete Frame Buildings

Author(s): Hitoshi Shiohara

Publication: Symposium Paper

Volume: 313

Issue:

Appears on pages(s): 1-10

Keywords: Seismic, design, concrete, beam-column joint

DOI: 10.14359/51689689

Date: 3/1/2017

Abstract:
A new concept of joint hinging developed in Japan is presented, which will be implemented in a new draft provision for beam-column joints in the New AIJ (Architectural Institute of Japan) Standard for Seismic Capacity Calculation. This paper discusses the key issues of the new draft provisions, with background, test data verification, theory and analyses with emphasis on why such a concept is necessary. The factors affecting joint hinging failure are discussed for seismic design consideration. Seismic collapse simulation were made by non-linear time history analysis for moment frames with BC joints failing due to joint hinging, to demonstrate the challenge of simulated strength degradation and severe pinching hysteretic behavior inherent to joint hinging. Draft equations to calculate the strength of joint hinging strength of BC joints are also introduced.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer