Title:
Experimental Evaluation and Analytical Simulation of Bridge Column to Footing Joints Connected Using Grouted Splice Sleeves in Seismic Regions
Author(s):
Chris P. Pantelides
Publication:
Web Session
Volume:
ws_2016_0814_Pantelides_EEASBCFJ.pdf
Issue:
Appears on pages(s):
Keywords:
DOI:
Date:
11/4/2015
Abstract:
ABC connections for concrete bridges are becoming more common in practice. It is the goal of this session to assess the current state of the art in research and practice regarding the use of ABC connections for the seismic design of concrete bridges.