Title: 364.11T-15 Managing Alkali-Aggregate Reaction Expansion in Mass Concrete
Author(s): ACI Committee 364
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 4
Keywords: alkali-aggregate reaction; maintenance; mass concrete; repair
DOI:
Date: 8/1/2015
Abstract: This Technote outlines the managing and expansion of the alkali-aggregate reaction in mass concrete.