Title: 330.1M-14: Specification for Unreinforced Concrete Parking Lots and Site Paving

Author(s): ACI Committee 330

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords: construction; curing; inspection testing; jointing; pavements;site paving; texturing.

DOI:

Date: 3/16/2015

Abstract:
This specification covers minimum requirements for the construction of unreinforced concrete parking lots on grade. Included are requirements for submittals, testing and inspection, concrete materials, embedded reinforcement at joints, jointing and sealant material, forms, subgrade preparation, subbase, placing, texturing, curing, jointing, tolerances, and opening to traffic. This specification does not cover requirements for pervious concrete.