Title: Structural Repair of Concrete Cracks

Author(s): Tom Murphy

Publication: Concrete International

Volume: 37

Issue: 4

Appears on pages(s): 52-54

Keywords: capping, delivery, ports, resin

DOI:

Date: 4/1/2015

Abstract:
Epoxy crack injection can be used for structural repair of cracks resulting from single occurrence events such as accidental overloads, vehicular impact, earthquake, restrained shrinkage, or excessive thermal differential in mass concrete. Typical applications include foundations, columns, beams, bridge decks, and bridge superstructures. The article describes elements that contribute to the successful and efficient application of epoxy crack injection—capping paste, injection ports, the injection resin, and the delivery system.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer