Title: Material Behavior of Ultra-High-Strength Concrete under Multiaxial Stress States

Author(s): Robert Ritter and Manfred Curbach

Publication: Materials Journal

Volume: 112

Issue: 5

Appears on pages(s): 641-652

Keywords: compression load; multiaxial load; multiaxial strength; multiaxial stress state; multiaxial stress-strain behavior; multiaxial stress-strain relationship; tension-compression-compression load; triaxial load; ultra-high-strength concrete

DOI: 10.14359/51687663

Date: 9/1/2015

Abstract:
To evaluate new fields of application of concrete structures in any processes where complex stress states occur, and to optimize concrete structure geometries regarding such applications, the material behavior of concrete under multiaxial loading has to be known. With the aim of determining the material behavior of an ultra-high-strength concrete (UHSC), 35 multiaxial stress states with primarily one tensile stress component are examined and the measured stress-strain curves are shown. Using the test results, the arbitrary parameters of a damage-based material law concerning the single-stress ratios are determined. To describe the material behavior for load-induced isotropic and orthotropic damage, an approximation of the calculated arbitrary parameters is deduced. These enable determining the material behavior of the investigated UHSC for any stress ratios. The prediction of the described material law is compared and discussed regarding the measured stress-strain curves and the maximum strength values from the tests.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.