Title: 364.10T-14: Rehabilitation of Structure with Reinforcement Section Loss (TechNote)
Author(s): ACI Committee 364
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 4
Keywords: concrete cover; corrosion; load-carrying capacity; rehabilitation; reinforcement; repair.
DOI:
Date: 7/1/2014
Abstract: Note: 364.10T-14 is only available in PDF format. Integrity of reinforcement is fundamental to the strength, ductility, and safety of reinforced concrete structures. Determining the necessity of additional or replacement reinforcement is a primary concern in rehabilitation projects containing corrosion of reinforcing steel.
Note: 364.10T-14 is only available in PDF format.
ACI Collection of Concrete Codes, Specifications, and Practices - Digital Subscription
ACI 562 PLUS Concrete Repair Subscription
Edit Module Settings to define Page Content Reviewer