Concrete of the Future: Overcoming the Challenges of Using Low Portland Cement Mixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete of the Future: Overcoming the Challenges of Using Low Portland Cement Mixtures

Author(s): Jussara Tanesi

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/23/2014

Abstract:
This session will showcase new advances in experimental, theoretical, and computational tools for characterizing cements, IBPs, natural minerals, and hydration and microstructure development in low-cement-content concrete binders. The technical content should be of great interest to both the academic and industrial community and of special interest to those involved in sustainable materials design and development, those who specify binder materials to be used in construction, and those who promulgate standards and codes for using low-cement-content concretes.