The Elastic Behaviour of Earthquake Resistant Reinforced Concrete Interior Beam-Column Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Elastic Behaviour of Earthquake Resistant Reinforced Concrete Interior Beam-Column Joints

Author(s): Briss, G. R.; Paulay, T; and Park, R.

Publication: Commentary Reference

Volume: 21

Issue: 29

Appears on pages(s):

Keywords:

DOI:

Date: 6/1/2011

Abstract:
Report 78-13, University of Canterbury, Department of Civil Engineering, Christchurch, New Zealand, Feb. 1978.