A Review of Recent Developments in ASTM Standard Specifications and ACI Guide Documents for Chemical Admixtures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Review of Recent Developments in ASTM Standard Specifications and ACI Guide Documents for Chemical Admixtures

Author(s): Charles K. Nmai and Bradley Violetta

Publication: Symposium Paper

Volume: 288

Issue:

Appears on pages(s): 1-12

Keywords: admixture, concrete, specific performance, standard specifica¬tion, state-of-the-art report, Type S.

DOI: 10.14359/51684225

Date: 9/14/2012

Abstract:
In this paper, the authors, who at the publication of this manuscript were the respective chairs of ASTM C09.23 and ACI Committee 212, review new developments and revisions to ASTM standard specifications and ACI guide documents for chemical admix¬tures through 2011. The highlights include the new Type S category in ASTM C 494/C 494M and its acceptance by agencies and specifiers, and the revamped and expanded ACI 212.3R-10 comprehensive state-of-the-art report.