FRP Laminates for Post-Earthquake Repair of Columns in 2 Hours
Author(s):
Murat Saatcioglu
Publication:
Web Session
Volume:
Saatcioglu.pdf
Issue:
Appears on pages(s):
Keywords:
seismic event, post-earthquake repair
DOI:
Date:
3/18/2012
Abstract:
This session will focus on case histories of rapid repair projects, challenges facing owners with a damaged structure, and the repairs required to use a structure after a seismic event. Emphasis is placed on projects with challenging timelines or conditions that have necessitated the use of unique technologies or approaches to facilitate the repairs.