Seven Principles for Sustainable Concrete Pavements
Author(s):
Thomas Van Dam, Peter Taylor
Publication:
Concrete International
Volume:
33
Issue:
11
Appears on pages(s):
49-52
Keywords:
design, materials, construction, recycle, life cycle
DOI:
Date:
11/1/2011
Abstract:
Concrete pavement sustainability can be accomplished by following the principles listed in the article. Each principle should be applied in terms of its interdependency with, and/or potential competition with, the other principles by using already available practical tools. However, there are still areas in pavement sustainability that need to be addressed or improved, including life-cycle systems to analyze economic, environmental, and social factors, and sustainable pavement rating systems.