Title: Autoclaved Alumina-silica Rich Industrial Waste Cement Systems Incorporating Reactive Magnesia

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/14/2011

Abstract:
The utilisation of industrial waste products as supplementary cementitious materials to produce blended Portland cement has increased worldwide in recent years. This study aims to investigate physical and mechanical properties of the addition of claybrick waste and reactive magnesia (MgO) as a low-emission alternative to ordinary Portland cement (OPC) binders in autoclaved calcium silicate based building products. The addition of clay-brick waste was found to be beneficial for drying shrinkage reduction but had an adverse effect on strength development. The addition of reactive MgO also showed a decrease in compressive strength but had some positive effects on bulk density. For the combined addition of clay-brick waste and magnesia an apparent synergy was observed which has been explained by the complementary physical and chemical effects.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer