Title: Long-term Strength and Serviceability of paving constructed with Pre-mix Recycled Aggregate Concrete

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
This paper discusses laboratory and field serviceability evaluation of recycled premixed concrete (RC) and conventional concrete (NC) used in construction of recreational facilities. The trials involved production and construction with recycled concrete made with 100% replacement of virgin coarse aggregate with recycled concrete aggregate (RCA). Two recreational facilities were investigated. The compressive strength of recycled concrete after 7years falls within 10% of the conventional concrete with the overall system serviceability remaining satisfactory for all facilities. Initial workability and placement of both RC and NC were found to be comparable. For standard cured specimens, higher drying shrinkage values, approx 25% are observed for RC with and without polypropylene fibres. However, corresponding in-situ NC and RC shrinkage measurements are comparable.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer