Title: 201.1R-92: Guide for Making a Condition Survey of Concrete in Service (Reapproved 1997)
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 16
Keywords: Durability
DOI:
Date: 10/1/1992
Abstract: Note: A newer version of this document exists. This document was replaced by 201.1R-08. This guide provides a system for reporting on the condition of concrete in service. It includes a check list of the many details to be considered in making a report, and provides standard definitions of 40 terms associated with the durability of concrete.
Note: A newer version of this document exists. This document was replaced by 201.1R-08.