Tensile Behavior of Fiber-Cement Hybrid Composites Containing Polyvinyl Alcohol Fiber Yarns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tensile Behavior of Fiber-Cement Hybrid Composites Containing Polyvinyl Alcohol Fiber Yarns

Author(s): Guodong Xu, Silvio Magnani, and Dave J. Hannant

Publication: Materials Journal

Volume: 95

Issue: 6

Appears on pages(s): 667-674

Keywords: glass fibers; polypropylene fibers; tensile properties

DOI: 10.14359/409

Date: 11/1/1998

Abstract:
This paper presents the results of a study of fiber-cement hybrid composites containing high-performance continuous polyvinyl alcohol (PVA) fiber yarns or rovings. Two types of hybrid composites were constructed, using fiber combinations of PVA and glass (either continuous glass or 38 mm chopped strand), PVA and Fibrillated polypropylene networks. The tensile stress-strain behavior of these hybrids was studied, showing that the bibers, when used in a hybrid form, could result in superior composite performance compared to their individual fiber reinforced cements. The PVA- glass hybrid composite allowed similar or more favorable composite properties to be achieved at a lower addition of the high elongation fibers compared to polypropylene-glass hybrids. In comparison with the hybrids containing glass fibers (i.e., polypropylene glass, PVA-glass), the PVA- polypropylene hybrid was less efficient at small strains (up to 1 percent), because of the high elongation of both fibers at small strains. However, the PVA polypropylene combination was advantageous in achieving high-ultimate composite strength because the PVA and the polypropylene could simultaneously contribute to the composite strength and because of the synergistic interaction between the two reinforcing fibers.