Title: Ten Years of Heavy-Duty Pavement in Western Canada

Author(s): Robert W. Piggott

Publication: Concrete International

Volume: 9

Issue: 2

Appears on pages(s): 49-54

Keywords: aggregates; bulk storage; cements; concrete pavements; highways; parking facilities; performance; roller-compacted concrete; General

DOI:

Date: 2/1/1987

Abstract:
Roller-compacted concrete (RCC) for pavements was first used in Canada in 1976 for a log-sorting yard in British Columbia. Since then, more than a dozen projects such as haul roads, bulk coal storage, and truck parking have been built in western Canada. The paving method offers the advantages of rapid construction with readily available road building equipment, use of lower cost marginal aggregates, and a pavement slab with properties similar to conventional concrete. Field performance has shown good resistance to freeze-thaw conditions. New uses in secondary highways and streets and in aircraft facilities are being contemplated.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer