Title: Model Study of Cracking of Prestressed Concrete Flat Plates

Author(s): P. R. Chadrabarti

Publication: Symposium Paper

Volume: 113

Issue:

Appears on pages(s): 133-156

Keywords: cracking (fracturing); crack propagation; flat concrete plates; models; post-tensioning; prestressed concrete; unbonded prestressing; tests; Structural Research

DOI: 10.14359/3003

Date: 4/1/1989

Abstract:
An attempt is made to study the crack formation, crack propagation, and the postcracking behavior until failure of four-panel prestressed concrete flat plates having two-way continuous parabolically draped unbonded post-tensioning tendons. The test specimens closely simulate the corner panels of an actual flat plate floor system having simple supports along the edges. The simple support system is similar to that provided by ledger beams or walls. The effect of added mild steel on the crack initiation, crack propagation, crack width control, and postcracking behavior is also studied. Recommendations are also made for further research.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer