Title:
Use of Cementitious Materials Other Than Portland Cement
Author(s):
Alan D. Buck
Publication:
Symposium Paper
Volume:
100
Issue:
Appears on pages(s):
1863-1882
Keywords:
alkali-aggregate reactions; blast furnace slag; concretes, evaluation; expansion; fly ash; mortars (material); portland cements; silica; sulfate attack; tests; Materials Research
DOI:
10.14359/2263
Date:
4/1/1987
Abstract:
Different amounts of fly ash, silica fume, or ground granulated iron blast furnace slag have been used with portland cement in an effort to prevent excessive expansion due to alkali-silica reaction or sulfate attack or both. The test methods used to establish optimum proportions were ASTM C 441 and ASTM C 1012. Once the optimum proportions were known, concrete mixtures were made and tested.