Influence of Superplasticizers, Polymer Admixtures, and SilicaFume in Concrete on Chloride Ion Permeability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Superplasticizers, Polymer Admixtures, and SilicaFume in Concrete on Chloride Ion Permeability

Author(s): S. L. Marusin

Publication: Symposium Paper

Volume: 108

Issue:

Appears on pages(s): 19-34

Keywords: admixtures; chlorides; concretes; epoxy resins; latex; permeability; plasticizers; plastics, polymers, and resins; silica fume; Materials Research

DOI: 10.14359/2147

Date: 8/1/1988

Abstract:
This paper summarizes the results of permeability studies that have been undertaken since 1979. The research used a test procedure developed during the NCHRP Project 12-19A, "Concrete Sealers for Protection of Bridge Structures", which was reprinted in 1981 as NCHRP Report No. 244. This test method utilizes 10 cm concrete cubes, and chloride ion penetration is determined at 4 depths after 21 days exposure to 15 percent NaCl solution. The test results show that lowering of water-cement ratio in portland cement concrete or presence of superplasticizers, polymer admixtures, and silica fumes are able to significantly reduce concrete permeability.




  