Title: Experimental Studies on Seismic Behavior of Reinforced Concrete Members of High Strength Concrete
Author(s): Sugano, S.; Nagashima, T., Kimura, H.; Tamura, A.; and Ichikawa, A.
Publication: Commentary Reference
Volume: 21
Issue: 11
Appears on pages(s): pp. 61-87.
Keywords:
DOI:
Date: 6/1/2008
Abstract: Proceedings, Second International Symposium on High-Strength Concrete, SP-121, American Concrete Institute, Farmington Hills, MI, 1990