International Concrete Abstracts Portal

  


Title: CMPM: Concrete: Microstructure, Properties and Materials

Author(s): P.Kumar Mehta & Paulo J.M. Monteiro

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 659

Keywords:

DOI:

Date: 1/1/2006

Abstract:
This textbook presents the art and science of concrete in a simple, clear, hands-on manner, focusing on the following: Cement and concrete are predicted to be the premier building material of the 21st Century; Includes unique diagrams, photographs, and summary tables; Updated to include new chapters on non-destructive methods for concrete; future challenges in concrete technology; an increased number of examples of concrete applications; and new developments in durability. Includes CD-ROM.


Product unavailable, please call +1.248.848.3800



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.