Influence of High Temperatures on Strength and Deformation of Concrete
Author(s):
H. Weigler and R. Fischer
Publication:
Symposium Paper
Volume:
34
Issue:
Appears on pages(s):
481-494
Keywords:
aggreagates; barite; compressive strength; concretes; deformation; heavyweight concrete; high temperature; moisture content; nuclear reactor containment; portland cements; quartz; research; slag cements; stress-strain relationships; thermal conductivity
DOI:
10.14359/18082
Date:
1/1/1972
Abstract:
This paper deals with the influence of high temperatures on the compressive strength and the deformations of concrete.