A Probabilistic Description of Structural Response

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Probabilistic Description of Structural Response

Author(s): Jack R. Benjamin and Haresh C. Shah

Publication: Symposium Paper

Volume: 31

Issue:

Appears on pages(s): 147-188

Keywords: beams (supports); building codes; columns (supports); failure; loads (forces); mathematical models; moments; probability theory; reinforced concrete; shear properties; statically determinate structures; statically indeterminate structures

DOI: 10.14359/17925

Date: 1/1/1972

Abstract:
The purpose of this paper is to provide the structural engineer with a simple probabilistic forecast of structural response. The procedure fits within all existing codes and is simple to understand and use.