Mixture Proportioning for Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mixture Proportioning for Mass Concrete

Author(s): John M. Scnalon, Jr.

Publication: Symposium Paper

Volume: 46

Issue:

Appears on pages(s): 77-96

Keywords: admixtures; aggregate gradation; aggregate size; air entrainment; coarse aggregates; compressive strength; cracking (fracturing); density (mass/volume); mass concrete; mix proportioning; portland cements; pozzolans; tensile strength; thermal properties

DOI: 10.14359/17870

Date: 1/1/1974

Abstract:
Very little has been published on procedures for proportioning mass concrete mixtures containing aggregates above 3 inches in size. The procedures currently in use by organizations deeply involved with mass concrete require a high degree of experience. The procedure described in this paper removes the necessity for this experience although an individual having knowledge of acceptable mass concrete workability should be available to evaluate the trial batch results and initial adjustments. The procedure described is intended primarily for proportioning concrete mixtures using aggregates above 3 inches in size but could be used to proportion concretes using smaller maximum size aggregate (1 and 2 inches).