Title:
Strength of Polymer and Polymer-Fibrous Concretes
Author(s):
T.S. Nagaraj, K.T. Sundara Raja Iyengar, and C.S. Viswanatha
Publication:
Symposium Paper
Volume:
58
Issue:
Appears on pages(s):
139-160
Keywords:
coarse aggregates; compressive strength; fiber reinforced concretes; impregnating; metal fibers; polymer concrete; synthetic fibers
DOI:
10.14359/17789
Date:
1/1/1978
Abstract:
With the continued research efforts, presently the techniques of production of polymer impregnated concretes have been fairly understood. Measured and evaluated mechanical properties and durability aspects of this material reveal that dramatic improvements are possbile thereby offering great potential to this material in building industry.